Spark plasma sintering can be used to make cylindrical shaped bulk samples, from metallic/ceramic/polymer powders. The samples are heated using Joule heating, which can be used to obtain a very rapid heating rate.
Max temperature: 2200°C
Max pressure: 50/100 MPa
Max heating rate: 100-1000°C/min
Mold size: 20-80 mm